It is shown that, in the course of rolling friction, the intensity of wear of hydrogenated specimens of high-nitrogen manganese steels is five times higher than for nonhydrogenated specimens. As the wear intensity increases, the color of the friction surface of the roller and the sizes of the wear products change. The outward appearance of nonhydrogenated and hydrogenated wear products is noticeably different (white and dark colors, respectively). The microhardness of the hydrogenated layer is equal to 7.6–8.2 GPa, whereas the microhardness of the layer of destroyed domains is 4.2–4.9 GPa. In the destroyed domains with signs of thermal seizure, we observe the elevated contents of carbide-forming elements (in particular, of molybdenum), which confirm the intensification of fracture in the investigated high-nitrogen steels under the conditions of rolling friction in carbide-enriched domains.






Similar content being viewed by others
References
O. I. Balyts’kyi, V. O. Kolesnikov, and P. Kaviak, “Tribotechnical properties of austenitic manganese steels and cast irons under sliding friction conditions,” Fiz.-Khim. Mekh. Mater., 41, No. 5, 55–60 (2005); English translation: Mater. Sci., 41, No. 5, 624–630 (2005).
V. V. Panasyuk (editor), Fracture Mechanics and Strength of Materials: A Handbook [in Ukrainian], Vol. 8: O. I. Balyts’kyi, O. V. Makhnenko, O. O. Balyts’kyi, et al., Strength of Materials and Durability of Structural Elements of Nuclear Power Plants, Akademperiodyka, Kyiv (2005).
V. I. Tkachev, V. I. Kholodnyi, and V. I. Vitvitskii, “Hydrogen fatigue of metals,” Int. Sci. J. Altern. Energy Ecоl. ISJAEE, No. 3 (11), 34–36 (2004).
O. I. Balyts’kyi and V. O. Kolesnikov, “Investigation of wear products of high-nitrogen manganese steels,” Fiz.-Khim. Mekh. Mater., 45, No. 4, 93–99 (2009); English translation: Mater. Sci., 45, No. 4, 576–581 (2009).
O. I. Balyts’kyi, V. O. Kolesnikov, and J. Eliasz, “Study of the wear resistance of high-nitrogen steels under dry sliding friction,” Fiz.-Khim. Mekh. Mater., 48, No. 5, 78–82 (2012); English translation: Mater. Sci.., 48, No. 5, 642–646 (2013).
V. A. Kolesnikov, “Investigation of the tribotechnical properties of high-nitrogen manganese steels after hydrogenation,” in: All-Ukrainian Conf. of Young Scientists “Present-Day Materials Science: Materials and Technologies,” Abstracts of Papers [in Russian], IPM NAN Ukrainy, Kyiv (2008), p. 130.
A. A. Deev, “Acoustic vibrations in the friction contact as a method for monitoring friction surfaces in the stage of running-in of the engines of internal combustion,” in: Bulletin of Esenin Ryazan’ State University [in Russian], No. 4 (29) (2010), pp. 28–31.
V. Ya. Matyushenko, “Wear resistance of hydrogenated metals,” in: Investigations of Hydrogen-Induced Wear [in Russian], Nauka, Moscow (1977), pp. 24–27.
P. V. Gel’d and R. A. Ryabov, Hydrogen in Metals and Alloys [in Russian], Metallurgiya, Moscow (1974).
L. Carlson, “Stainless steel: past, present, and future,” Suvirinimas. Welding–Journal Weld. Technol. Mater., No. 1 (4), 17–20 (2004).
Author information
Authors and Affiliations
Corresponding author
Additional information
Translated from Fizyko-Khimichna Mekhanika Materialiv, Vol. 50, No. 4, pp. 110–116, July–August, 2014.
Rights and permissions
About this article
Cite this article
Balyts’kyi, O.І., Kolesnikov, V.O., Eliasz, Y. et al. Specific Features of the Fracture of Hydrogenated High-Nitrogen Manganese Steels Under Conditions of Rolling Friction. Mater Sci 50, 604–611 (2015). https://doi.org/10.1007/s11003-015-9760-9
Received:
Published:
Issue date:
DOI: https://doi.org/10.1007/s11003-015-9760-9